yes, u can use 318 in place of 316L
On Tue, Aug 30, 2022, 1:05 PM Manish Tripathi <manish.tripathi.mech@gmail.com> wrote:
Dear Members,I have doubt that, If WPQR qualified on Group 8.1 with filler ER316L, Can we use to weld by ER308L or ER318 for Group 8.1 material, as per 8.4.4 of EN 15614-1 Level 2. provide all variable remain same.Regards,Manish Tripathi--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/28325c34-8fe4-4f95-82f9-e83aa98f3650n%40googlegroups.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNvhN%2BNw2dCwJ%2Bq34iPvBy3b7M1D_MoL%2BS3%3D5ACpFkU4w%40mail.gmail.com.
Comments