Thursday, September 1, 2022

Re: [MW:33419] EN 15614-1 Filler material changes & restriction

No same fillerwire required

On Tue, 30 Aug 2022 at 13:05, Manish Tripathi <manish.tripathi.mech@gmail.com> wrote:
Dear Members, 
I have doubt that, If WPQR qualified on Group 8.1 with filler ER316L, Can we use to weld by ER308L or ER318 for Group 8.1 material, as per 8.4.4 of EN 15614-1 Level 2. provide all variable remain same.
Regards,
Manish Tripathi

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/28325c34-8fe4-4f95-82f9-e83aa98f3650n%40googlegroups.com.
--
Pravinkumar kurade

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM02rkeYDzKitAHNwbyZqLcxAZDuVARXq%2Bv6nfx2F-34MTe4CA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...