Thursday, September 8, 2022

[MW:33452] Double V or Single J Groove

Dear Experts,

Awaiting your valuable suggestions to select the groove design, my conditions are as follows.

MOC : SA 516 Grade 70
Vessel Dimensions : 2438 mm ID x 70 mm Thickness
Welding Process : SMAW + SAW (Narrow gap welding machine) 

Thank You & Regards
Williams P Wilson
QA/QC Engineer
Please consider the environment before printing this message

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHBxnQ6r-NZuuSC2YLsMioThLsU1fHxZtowqJK5M_Rn1fZH-5g%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...