Re: [MW:33228] Hardness Issue on weld metal

Dear,

I am not clear, could you explain in detail

Thank You & Regards
Williams P Wilson
QA/QC Engineer
Welding Inspector (CSWIP 3.1)
Cell: (+968) 94600828
P Please consider the environment before printing this message


On Wed, Jul 13, 2022 at 3:45 PM 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Supported by Simulation coupon as Tensile strength also reduces.

Thanks & Regards

J.Gerald Jayakumar




On Wednesday, 13 July, 2022 at 05:07:59 pm IST, pradip kumar Sil <pradipsil@gmail.com> wrote:


Re PWHT you can do to minimize hardness

On Wed, 13 Jul 2022, 16:52 williams p wilson, <williamswilsonp@gmail.com> wrote:
Dear Experts,

During the PQR qualification of ASTM A 519, Grade 4130 , Pipe 3" x Sch XXS material hardness value in SMAW weld metal area observed in b/w 247 to 283 HV.

The required value is in blw 201 to 241 HV, Base metal hardness also is in the same range.

Preheat temperature : 200 ° C
Interpass temperature : 300 ° C (Max)

Stress relieving details as follows,
600 ° C ± 10  ° C, Holding Time : 01 Hour
Cooling Rate : 150 ° C / Hour
Heating rate : 150 ° C / Hour
Unrestricted heating up to 300 ° C
Controlled cooling upto to 300 ° C

Please reply with your valuable comments to reduce the high hardness observed in the weld metal.

Thank You & Regards
Williams P Wilson
QA/QC Engineer
Welding Inspector (CSWIP 3.1)
Cell: (+968) 94600828
P Please consider the environment before printing this message

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHBxnQ7aeEfBAfaiPFbU12cS97SJOSG3-TRyHfBcbFHRzkZnGQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8kvAiVC5NKGjRMnRgivK-d0C9r2yamTUBMdWTWu4G3y7A%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/259161802.482199.1657712663381%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHBxnQ6ooM70feeYoCnojUJ3_rvvWP4JrjjhD7ahwgCjCjsvEA%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...