Dear Expert,

we have some pipes of 316 material all pipes are off cut and heat identification is not available on these pipes. MTC type requirement is 3.2 also we have not MTC. what is the Procedure to certify the material as per the 3.2 type requirement? 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c083e4ed-c02a-49dc-b2a4-c3d8c8c8c738n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS