Re: [MW:33309] Different between E8018-b2 / E8018

Dear Mr. Hari,

Thank you for your question.
 I am totally agreed with Mr. sham reply.

Regards,
Binit Kumar(Welding Inspector)
Doosan Power Projects Pvt. Ltd.
NTPC Barh, Bihar

On Mon, Jul 18, 2022 at 5:12 PM Hari krishna <autocadstudent23@gmail.com> wrote:
Dear sir

what is the difference between E8018-b2 / E8018, where there will be major differences or minor? 

when will this difference be seen seriously?

Thanks All :)


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/412ec4ee-f360-49a3-a610-6b7019baceb6n%40googlegroups.com.


--
BINIT KUMAR
+918717929495

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJ0ob9DeDonR-75yYZHHiqc0fMrNS_0iwxYGHsfuiGxp%2Bhez0g%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...