Yes, you are correct ASTM A380 is only for pickling and passivation.

On Tue, Jul 26, 2022 at 11:42 AM Anilkumar G <akg.nitt@gmail.com> wrote:
Dera Sajeed

A380 describes only pickling & passivation procedures in detail I believe, not about painting. Please correct me if I am wrong.

Regards
Anilkumar

On Tue, Jul 26, 2022 at 2:05 PM sajeed zaheer <sajeed7674@gmail.com> wrote:
ASTM A 380

On Tue, Jul 26, 2022 at 11:19 AM Anilkumar G <akg.nitt@gmail.com> wrote:
Dear Experts

Do we need pickling and passivation of SS surfaces before painting them? Could you please suggest any specification relevant this requirement?
The parts are SS cast valves requiring painting.

Regards
Anilkumar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/754e0d61-54e1-420e-ae4b-f92593266f5en%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFycdMz9RbXVXteXk%2B3MvOj%3D%2B2ftw-bu-N9jAx1tsvtrz3L7Gw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKMJiNVwvB2pPdDwc2BtMtbebK%3DJCXF9WBt1ZR%3DPTj-%2BOjymLQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFycdMyDQvXQFVvEGCtO%3DV%2BTXgtu9fcU1NchzwYUZ%3DyKAqkeTw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...