Re: [MW:33248] SA-516 Gr 70

E 7018 is the correct one. The sail test certificate mentions the observed values nothing to worry about it. 


On Fri, Jul 15, 2022 at 12:31 PM Kishore S <kishore.sk002@gmail.com> wrote:
Dear sir 

what are the step to find an electrode for SA516 gr 70 in the internet they have mentioned E7018 but as per the SAIL TEST CERTIFICATE tensile strength is 79ksi so what electrode do I have to use   

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ab5513fa-c564-40ce-953a-f67e68a3ea03n%40googlegroups.com.


--

Ramesh Babu Balaram

Corporate Head, Quality

The Oriental Towers, No. 461, 1st Floor, 17th Cross Road, 4th Sector,

Sector 4, HSR Layout, Bengaluru, Karnataka 560102.

M 9840531355  E rameshbabu.b@zetwerk.com  W zetwerk.com

App Green Footer Image Please consider your environmental responsibility. Before printing this e-mail message, ask yourself whether you really need a hard copy.



This information may be confidential and/or privileged. Use of this information by anyone other than the intended recipient is prohibited. If you receive this in error, please inform the sender and remove any record of this message

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHJfB2n1uTs2QnY%2Bm0TJw0dCc9aRpROrXxdsOTmesAVJx0D6jw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...