Re: [MW:33244] WELDER QUALIFICATION REQUIERMENT

Choose a higher thickness pipe say 20mm wherein you can weld GTAW 5mm (2t) and SMAW 15mm with minimum 3 layers so for SMAW he will be qualified for unlimited thickness and say GTAW 10mm/

Thanks & Regards

J.Gerald Jayakumar



On Thursday, 14 July, 2022 at 05:09:42 pm IST, Adnan Ziad <adnanziad49@gmail.com> wrote:


In our case he weld 5 mm gtaw + 9.27 mm smaw 

Can i qualify him directly on the two wps 

On Thu, Jul 14, 2022, 12:09 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:
What you have mentioned is Basemetal thickness but in Welder qualification only weld metal thickness is an essential variable qualified from 0 to applicable weld metal thickness for each process, BM thickness is unlimited

Thanks & Regards

J.Gerald Jayakumar




On Thursday, 14 July, 2022 at 01:18:52 pm IST, QA/QC <adnanziad49@gmail.com> wrote:


Dear Experts

i have two wps's for piping cs/ltsc welding with the asme b31.3 ans sec 9  one thickness range is 3 to 20 mm and the second is 20.01to 31.22  pwht requiered .the two is GTAW+SMAW

i have a welder qualify in test coupon 6'' 14.27 mm 

my question is this welder will qualify to weld in the two wps or we should make another qualification for him seperately 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/083762d2-dd64-482a-85e9-0e4f7aa4e14bn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1357071013.761925.1657796938751%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACbfGKfUAWSWQBvotP2q78PrFFKk5eqBCem3vh-a2pvEbvbAqQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...