Monday, July 18, 2022

Re: [MW:33271] Different between E8018-b2 / E8018

Dear Hari

E 8018-B2 is a low alloy CS Electrode. B2 in this represents the alloy content in the electrode. Please refer ASME SEC II C PART- SFA 5.5 for details of various electrodes in the low alloy CS. As per my knowledge E8018 is not mentioned in the standard which means this electrode is not available. 

Regards
SHAM SHAHABUDDIN
QC INSPECTOR - WELDING
HANBO ENGINEERING & CONSTRUCTION
MARJAN INCREMENT PROGRAM ( MIP - PKG 6 )
MOB: +966-572066357


On Mon, Jul 18, 2022 at 2:42 PM Hari krishna <autocadstudent23@gmail.com> wrote:
Dear sir

what is the difference between E8018-b2 / E8018, where there will be major differences or minor? 

when will this difference be seen seriously?

Thanks All :)


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/412ec4ee-f360-49a3-a610-6b7019baceb6n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAyAb6PoiWbyjYBev_L5bmhth%2BVUemGuaFcE8PVo29e5wQ8i6Q%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...