Re: [MW:33324] CS material, E70S2- Welder qualified , can he weld SS 316 material & Duplex, Super duplex material with E70s2 qualification ? or he should be qualified by separate SS 316 & Duplex ,SDSS material ?
Check the filler no of both welding consumble if both are same we can use it,
On Fri, 29 Jul, 2022, 11:43 am Madheswaran s, <madhes.sss@gmail.com> wrote:
Dear Experts,CS material, E70S2- Welder qualified , can he weld SS 316 material & Duplex, Super duplex material with already he has E70s2 qualification ? or he should be qualified by separately for SS 316 & Duplex ,SDSS material ?Thanks,Madheswarn.S--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2d44c76c-a78f-402e-80a7-0616f1c9ca0an%40googlegroups.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzo-kvMWkYWT0y0z43%2BevR_r8HtviRGH2LFTGUvjvCSPwttUw%40mail.gmail.com.
Comments