Friday, July 15, 2022

Re: [MW:33253] SA-516 Gr 70

SA 516 Gr 70 Means 70KSI  or 490 MPa is minimum UTS required was per SA 516. for these plates.

Compatible electrode  is E7018  as 
minimum UTS of this electrode is 70KSI minimum or 490MPa minimum. 

This is Welding and Material Technology compatibility and acceptable to Code requirements. 


On Fri, 15 Jul 2022, 11:53 Kishore S, <kishore.sk002@gmail.com> wrote:
Dear sir 

what are the step to find an electrode for SA516 gr 70 in the internet they have mentioned E7018 but as per the SAIL TEST CERTIFICATE tensile strength is 79ksi so what electrode do I have to use   

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ab5513fa-c564-40ce-953a-f67e68a3ea03n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3OgfHiZLxwN%3DXQ85w%2BwFHmi5%2B3YFt%2BD37Mh8vRWo%3Duk2w%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...