Re: [MW:32115] API 650

Ref: API 650: 8.1.5 Radiographic Standards
Welds examined by radiography shall be judged as acceptable or
unacceptable by the standards of Paragraph UW-51(b) in Section
VIII of the ASME Code

On Fri, Jan 22, 2021 at 2:17 PM chitko khaing
<chitkokhaing2009@gmail.com> wrote:
>
> Dear all
> I am chit ko from Myanmar. i want to know " API 650 RT acceptance Criteria" refer to ASME VIII Division 1?
>
> --
> https://materials-welding.blogspot.com/
> https://www.linkedin.com/groups/122787
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9483308e-f4ab-4851-8f1e-e0565a3f19ben%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAE4dwYNHydZmsu4uNDsHLfOTerOTfHjF6T3XaW2itqayf7Yc1g%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...