Correct,
Refer API RP 945 for amine service.
PWHT is required and hardness control is required.

On Mon, Feb 1, 2021 at 8:43 AM PSS <mechselastine@gmail.com> wrote:
Experts

Client Requirement : Vessel shall be PWHT. Production Weld deposits hardness shall not exceed 200HBW after PWHT. Carbon steel welds shall comply with NACE STD SP0472 para. 2.2 & 3.3

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a024d874-aeff-4042-afd5-cf7b8a6e2a62n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAA_HBVv4h2ZAFpoDztCeWOZA8hYPq9GZ-BOh9Vpi2KSZWzBkZg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...