Use ENi CI electrodes with pre heating @200 Deg C
Use Multipass welds
On Thu, Mar 25, 2021 at 7:13 AM QA/QC <adnanziad49@gmail.com> wrote:
Dear masterin our project we have a leak in fire water service and i want to know the repair procedure for the pipeductile iron C151A21.51electrode rod using for andf procedure if possible--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bd7269bd-a954-4c54-a816-2c3c45a84f3bn%40googlegroups.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3MDO5fX-2OUgkFm43xc3GFUdxTJL-W7tE%3DeE2pewmeoSQ%40mail.gmail.com.
Comments