Re: [MW:32076] SMALL DIAMETER PROCEDURE QUALIFICATION AS PER ASME SEC IX

I think you are complicating your life more than necessary, to do the bending and tension tests that your PQR needs per ASME IX requirements, you can use a tube of greater diameter and thickness of the same P number or if you like the same material, that will allow you to do your tests without any problem or setback, that is completely valid and design and write your WPS according to: thickness (0.89mm) and small diameter (6.35mm), your laboratory tests do not have to be strictly under these parameters: thickness (0.89mm) and small diameter (6.35mm).
Greetings!.

El mié, 17 mar 2021 a las 21:07, Vishwas Keskar Welding Manager WELDING (<vvkeskar123@gmail.com>) escribió:
Dear Experts ,

PQR is to be qualified  for 
6.35 mm OD X 0.89 mm thickness 
Welding Process - Autogenous Fusion - GTAW Orbital WELDING 
Code - ASME SEC IX 
Material - SA 213 TP316L
Tensile test - 2nos 
Face bend test - 2nos
Root bend test - 2nos 
Full section tensile test is carried out and found satisfactory 

Bend test samples can not be prepared due to less thickness(0.89mm) and small diameter (6.35mm).  Pipe Sectioning  as per permitted by ASME  for small diameter is tried  but could not do it .
When tried to  cut into sectioning for  bending test piece preparation , pipe is getting bent and sectioning is not possible .
 Experts , Pl. help how to go about bend testing or any other way forward 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6e39e586-dc33-4c22-a83e-30255b37a887n%40googlegroups.com.


--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SUMMIT MÉXICO - TPI

https://www.linkedin.com/in/summit-m%C3%A9xico-tpi-760047137/

Móvil +52 1 812 352 4606

Skype: jjjimeneza





--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5ZurL%3D5DBGCFT2qX6HuQ-rR%2BxGZxDyahtyvMgn17bvK17Lbg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...