Which code permits to do wpq like this?

On Wed, 17 Mar 2021, 13:52 TDK YOKESH, <tdky167@gmail.com> wrote:
Dear experts,

I am qualifying 2 welder on 20" pipeline. One half welder by welder A and other half welder B.  The RT result shows Welder A side failed and Welder B side passed.
Query : Both the welders are rejected as the coupon has failed or should I consider welder A and welder B passed.

Any code reference or interpretation on similar case will be helpful. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKT-TuovOFQLQmMRN17eosER4WP1cMtcEWQb%2BRhiAnvmaEG7EA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGnSN%3DJdgHuaNL9SRea-Sx_8rL%3DViKO0JFc522b_y5fbbRuxDw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...