Tuesday, March 16, 2021

Re: [MW:32064] welding of HARDOX 500 to CS Plates

Dear sir,

It depends on the plate thickness because if the thickness of hardox 500 is more in that case chemical composition changes due to hardness. (like NI for less thick ni-0.2 for high ni-1.5, mo .25 to .6, cr 1 to 1.4)
Regards

Lalit Vadadoriya

Mob.9377072930


On Mon, Mar 15, 2021 at 9:12 AM Hani Al Masry <hanyonalfy@gmail.com> wrote:
Dear All 

which electrode can be used for welding of HARDOX 500 to CS Plates 

Regards,
H.A 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKOkEzc0WxOA%3DF3ft98VJOenqO_X6SN0WMmJMVNeOE4Va9d0pw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKjb_1L0CE8sEys%2BGAti3eysKM%2Bcnc-7fxicBu5aH37XuNtC2g%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...