THANKS , WHAT IS THE EQUIVALENT TO USE SMAW OR FCAW? 

DO WE NEED ALSO TO DO BUILD UP (HARDFACING) FOR THE WELDING FINAL WELDING LAYERS AFTER JOINING? 

Regards,
H.A 


On Mon, Mar 15, 2021 at 10:17 AM Rahul Rathod <welder.tigarc6g@gmail.com> wrote:
For joining or build up?

On Mon, 15 Mar 2021, 9:12 am Hani Al Masry, <hanyonalfy@gmail.com> wrote:
Dear All 

which electrode can be used for welding of HARDOX 500 to CS Plates 

Regards,
H.A 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKOkEzc0WxOA%3DF3ft98VJOenqO_X6SN0WMmJMVNeOE4Va9d0pw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANaNbfk-6HupPMwqAmGETuqG8e%2BNxphHyG3FMQGR4c-2ARnVgg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKOkEzd_hwktQcSqK6rDF8uE7UEGFf575SFbRvNPD_t4CHJ4Og%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...