Monday, March 15, 2021

Re: [MW:32060] welding of HARDOX 500 to CS Plates

Dear Sir,

As per the Hardox manufacturer recommendation, you may go for AWS E307 type of welding consumable without any preheating. 


Regards,

Aditya Gujar
Essen Welding Alloys Pvt. Ltd.,

On Mon, Mar 15, 2021 at 9:12 AM Hani Al Masry <hanyonalfy@gmail.com> wrote:
Dear All 

which electrode can be used for welding of HARDOX 500 to CS Plates 

Regards,
H.A 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKOkEzc0WxOA%3DF3ft98VJOenqO_X6SN0WMmJMVNeOE4Va9d0pw%40mail.gmail.com.


--
--
 
Aditya Gujar
Sales Manager
Essen Welding Alloys Pvt. Ltd.,
Pune, India.
 
Tel: 91 20 65781493
Mob: 91 9850958075
---

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB89cpBiAh7gabtYr08TokmmbZGU_xKW1T7b-e6Gj5Z3GdvuMw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...