Monday, March 8, 2021

Re: [MW:32035] Welder qualification

Please find below the Essential variables for GTAW welder qualification. Any change in one essential variable as dictated by the other relevant portions of the code require new welder qualification.

Inline image


Thanks & Regards

J.Gerald Jayakumar




On Sunday, 7 March, 2021, 12:56:28 pm IST, Ganesh Muthurajan <qceng.mg@gmail.com> wrote:


Hi gentlemen 

I have doughty in welder qualification. 


The welder having two jcc.

1. GTAW - OD - 1inch, Thickness- 11.08mm, P no. 34, F no 34

2. GTAW+SMAW - OD - 2 7/8 Inch, Thickness - unmimited, P No. 1, F no. 6.


Now my doubt is 

The welder can weld ?

1. CuNi - 12.7 mm thickness 

2. CS - 1" OD

How? If not why?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM0EmF%2BwEcrFhPnEXJFvizXJo9SePFQLKS1%3D-tBE2c_6Q_h6tw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...