Looks Good, Flat & G may be included in the Arrow side.

Thanks & Regards

J.Gerald Jayakumar




On Sunday, 7 March, 2021, 12:57:28 pm IST, EmaD FaRaHanI <emad.farahani@gmail.com> wrote:


Dear all,
can you help me what are the problems with this welding symbol?
Details: the pipe outside diameter was 20" with a wall thickness of 1.5 inches thick. The architect wanted the welds to be ground flush on the outside surface, where as the field joints were to be made using permanent steel backing rings. The Engineer selected the following welding symbol for showing the field welds using a backing bar (ring).

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABtwbJGP%3DATezfC38Z1k8k8XrLhJRTwhd%2BaUzwTwrkyehpOc5Q%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...