Re: [MW:32024] RE: FCAW substitute for SMAW in offshore platforms

GMAW with Pulse is the best choice with 95Ar+5Co2

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Sat, Mar 6, 2021 at 3:32 AM <pgoswami@rogers.com> wrote:

Hi

FCAW is one of the approved welding processes for offshore construction. Often restrictions are imposed by the end user/client. You need to go by what your project/client specification calls for. Here're some industry specific documents for your reference. GMAW is also a reliable process, however type of the process, i.e.  short circuit/ globular/spray arc decides the application and the effectiveness of this technique.

By and large of the processes are far more accomplished than what they were ,15-20 years ago.

 

Hope these attachments will provide the general insights on your query.

 

Regards.

 

 

 

Pradip Goswami.P.Eng, IWE.

Independent  & Consulting Welding & Metallurgical Specialist

Saudi Aramco Approved Designated Welding Engineer(DPWR)

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@rogers.com,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

From: EmaD FaRaHanI <emad.farahani@gmail.com>
Sent: March 5, 2021 12:01 PM
To: materials-welding@googlegroups.com
Subject: FCAW substitute for SMAW in offshore platforms

 

Dear All,

I want to replace SMAW in the fabrication of offshore platforms, top side section.

In this regard, FCAW is selected mainly for most of the welds, to increase the speed of fabrication.

May I know:

1- Is FCAW the right choice? how about GMAW?

2- In the case of FCAW, which electrode with a 3.2mm size is proper for all position welding in offshore platforms? mainly high strength steels

 

Regards,

E.F


Virus-free. www.avg.com

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAuAAAAAAAAABVPzeizzeRJsiPziIE5jXQBAMO2jhD3dRHOtM0AqgC7tuYAAAAAAA4AABAAAACUA%2BTK4cT5SKO3larXFGO0AQAAAAA%3D%40rogers.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOC0Mw04raQR1ZAyrxYhYnC3TiKXb_r7%3D-9EM2zccy_pw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...