Wednesday, March 31, 2021

[MW:32131] interruption limitations to stop welding

Dear All ,

  In our Pressure vessel project 10mm thickness plate they using (GTAW+SAW) process , They have welded GTAW with 4 mm of 10mm thickness and leave open for 1 days .. I like to Know what is the interruption limitations to stop welding Limits for <19mm thickness 

Please send me code documents 

--