Dear Expert,

Find the below chemical composition values as per PMI, unfortunately we do not have any Test certificate and traceability. Can you please provide an update.

Carbon Steel
Fe 97.8%
Ti 0.85%
Co 0.62%
Mn 0.50%
Zn 0.17%
Cr 0.06%

Thanks in advance
--
Regards
Dhanabal Jalachandran

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPLwtDc-dvTWafoz%2B99A8YCc0f1HQCRfBctVEuYCiyf3i-rhVw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...