Wednesday, March 24, 2021

[MW:32090] ductile iron welding procedure

Dear master 

in our project we have a leak in fire water service and i want to know the repair procedure for the pipe 

ductile iron C151A21.51 

electrode rod using for andf procedure if possible 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.