[MW:32082] Demineralized Water For Solution Annealing

Dear Experts,

Good day.

Regarding the mentioned subject we are doing solution annealing for ASTM A 240 Gr 321H piping spools as per the client requirement. Kindly clarify that the re-use of quenching water, whether it is acceptable or should be changed for every heating cycle.

Thanks & Warm Regards,

KARTHIKEYAN  M.
Mobile:+966-501176985,
P Save A Tree - Please do not print unless really need

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAL7K%3D_Lr9V8G0NoYW0X4-mnkJ6bx%3DUDaVpkCUH%3DNWqpGyJGxgQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...