Dear All,
I want to replace SMAW in the fabrication of offshore platforms, top side section.
In this regard, FCAW is selected mainly for most of the welds, to increase the speed of fabrication.
May I know:
1- Is FCAW the right choice? how about GMAW?
2- In the case of FCAW, which electrode with a 3.2mm size is proper for all position welding in offshore platforms? mainly high strength steels

Regards,
E.F

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABtwbJE2HAz97vDLBZLea6Rd8vjfo64-gngvW4WXMDyiE5Rc-w%40mail.gmail.com.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...