Wednesday, June 6, 2018

[MW:27938] minimum leak path calculation for tube to tubesheet joint

dear experts,
i require the calculation of the minimum leak path calculation for tube to tubesheet joint.
below are the deatils:

Full strength weld Joint

Design temperature: 150 °C

Tube sheet Material: SA 266 gr.2

Seamless Tube Material: SA 266 gr.2

Tube OD: 19.05 mm

Tube Thickness: 1.91 mm

--