RT-1 is full radiography. And there is a difference between full radiography vs 100% radiography. If 100% radiography is required then you need to provide lip joints for all nozzle to shell junctions which can be radiographed. 
Coming to the main question, UT is not required as it's not a mandatory requirement. You need to perform PT/MT for nozzle to shell junctions, Soap bubble test for RF pads.
UT can be performed in lieu of RT on lip joints if 100% RT is a requirement. 

On Mon 25 Jun, 2018, 5:53 PM Muhammed Ibrahim PK, <ibratech@gmail.com> wrote:
Dear Experts,

I would like to get info on following scenario.

Design code : ASME Sec : VIII Div. I

RT requirement : RT1

Service : Not Sour / lethal /  cyclic etc (Sulfur recovery Incinerator package).

The vessel having set in type nozzle with full penetration groove. This nozzle to shell weld cannot be radio graphed (Not lip type).  Is it required to do UT of nozzle to shell weld (Category D) joints for this vessel  if RT is not possible ?.
 

Please see attached joint configuration.


Thanks & Regards
Muhammed Ibrahim PK

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...