Sunday, June 24, 2018

[MW:27978] Re: Required Hydrotest pressure Drop calculation due to Temperature drop

You can use the below formula,

P1/T1 = P2/T2.

As per my calculation for your reading, 28.05 bars is acceptable.

Regards,
Madhan. S


On Tuesday, June 5, 2018 at 8:15:54 AM UTC+3, sankar krishnan wrote:
Dear Brother

We have facing problem at Hydro test , Pressure Drop same time Temperature also Drop , Now our client asking Drop calculation according to temperature drop 

We are Doing Holding time for 1 Hour at our project , Due to welded joints are full painted 

4" Line sch -120

Start Hydro test :
 Test pressure =29.4 Bar
  Temperature=35.1C

After 1 Hour 

End of Hydro test :
Test pressure =27.4 Bar
 Temperature =33.5C

I have know Temp drop will be equal to pressure Drop , Now My question how we can drive formula and shows that above hydro test accepted 

Borthers , I need pressure change for a change in test water temperature Calculation if any one can drive formula and send me or you have any excel formula please share in our group 

Best regards
Sankar.k
Welding Inspector 
Iraq 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...