[MW:28007] Re: reg: Maximum interpass temperature in a WPS

Update:  deleted in 2017 edition

On Tuesday, November 29, 2016 at 6:34:57 AM UTC+4, Prince C thomas wrote:
Dear Sir's,

Kindly reply to  my below query:

We have project approved WPS with following details:

Material Spec: ASTM A106 Gr.B

P no:1/Group no:1

Material thickness: 1.5 -14.22 mm

Welding process: GTAW+SMAW

GTAW-Filler wire : ER 70S-2

SMAW-Electrode: E 7018

Preheat - 10 deg minimum

Interpass temp: 200 Deg C Maximum

In the PQR: pre heat temperature:38 deg C

                  Interpass temperature: 68 deg C maximum



Since interpass temperature is not a essential variable (Impact test is not applicable); but still our client is asking to recheck the max.interpass temperature value ( 200 Deg C) in the WPS. How to convince client to get approval on the same?






--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...