Saturday, June 23, 2018

Re: [MW:27976] Electrode for MS to SS409

hi!

use only 309 Electrode.
Regards

On Wed, Jun 20, 2018 at 5:49 AM, 'Sankaran Sp' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear friend,

you can use E 309Mo or Nickel base electrode for welding of MS to SS409..
 

Regards,
Sankaran.SP
Welding & Metallurgy expert



On Wednesday, 20 June, 2018, 4:12:16 PM IST, santosh nayak <san2.nayak@gmail.com> wrote:


Please can any one suggest the electrode for MS to SS409.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...