Re: [MW:27987] NACT plate

Dear Jayesh:

NACT is Normalizing and Accelerated Cooling & Tempering. The Accelerated cooling is critical (by air blasting or quenching) but it all depends on final results. If mechanical properties of the final product meet your min. requirements, there should not be anything to worry about. Accelerated cooling is crucial for preventing grain growth and if you decide to just proceed with cooling in air, you might run into problems with your final assembly.

Regards 

Ramin  Kondori
Sr. QA/QC & Welding Engineer
-----------------------------------------------------------
PG-Dip. in Welding Engineering (IWE  AT  0070)
BSc. in Civil Engineering (IUT)
BGAS Painting Inspector
ASNT Level I&II
                        
IIW-Logo-Colour-small


On Tue, Jun 26, 2018 at 3:07 PM Jayesh Parekh <jayeshparekh34@gmail.com> wrote:
i purchase SA387 plate in NACT condition. But in my fabrication process i have to give one intermediate normalizing. So, this intermediate normalizing cycle also follow NACT cycle ? Or i only normalized and then tempered material, it will ok or Not ?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...