Re: [MW:27970] Electrode for MS to SS409

On 20-06-2018, san2.nayak@gmail.com via materials-welding+bncBCCPPBVV4AOBBAW7VDMQKGQEEATIGNI@googlegroups.com wrote:

try  StainTrode  D or XHD 2222 of EWAC 
---

with best regards

= s p raman=
J.Suryanarayanan
7, Biplabi Rash Behari Basu Road
Kolkata - 700001
Phone no 033 22302751/22103478
Direct  Phone 033 40010934
email: jsn@cal2.vsnl.net.in
Please can any one suggest the electrode for MS to SS409.

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...