Corrosion causes half of hydrocarbon spills in Colorado


Corrosion causes half of oil, gas flowline spills

That means that as much as a quarter of all spills in the state reported to the Colorado Oil and Gas Conservation Commission relate to flowline corrosion. Mark Schlagenhauf, engineering integrity supervisor for the commission, said flowlines account for 40 to 50 percent of all spills that energy companies report to the agency.
Flowlines are pipelines running directly from wells, typically to the point of gas metering or where tanks collect produced oil. Flowlines also may carry water associated with oil and gas development. The commission doesn’t regulate other pipelines, such as gas gathering and transportation lines moving gas farther downstream.
The commission’s newly formed Engineering Integrity Group has undertaken a flowline audit program, and since the start of 2016 it has conducted 30 audits, mostly focused on larger companies operating in the Denver Julesburg Basin, North Park, and in western Colorado’s Piceance Basin.
The audit has its roots in direction the commission received several years ago from the Legislature to develop and implement a risk-based strategy for inspections in the state. An ensuing consultant’s evaluation of 1,638 spills reported from January 2010 to August 2013 found that 78 percent occurred during production.
The Legislature then appropriated funding for the Engineering Integrity Group, which includes a supervisor, engineer and field inspector. The group has turned its initial attention to flowlines, the source of the majority of production-related spills.
The audit’s review of causes reported from September of last year through February of this year showed that 48 percent of the spills resulted from corrosion, Schlagenhauf said. He said that number is consistent with other time periods evaluated since his group’s formation in late 2015.
“There’s a lot of old metal pipe out there,” he said.
The review found that natural events like freezing accounted for about 20 percent of the other flowline spills, with the remainder resulting from excavation damage, operator error, equipment failure, and weld or joint failures.
Identifying causes can help zero in on preventative measures such as more frequent adding of corrosion inhibitors to pipes, replacing older pipes and burying lines below the freeze line underground.
The commission requires flowlines to be pressure tested before being put in service, and then annually. The auditors have reviewed more than 3,800 pressure tests, audited more than 2,800 wells and done more than 400 flowline-related inspections.
Schlagenhauf said while the audit has resulted in some notices of alleged violations, typically in response to a spill, its focus has been on helping companies improve prevention efforts.
Preventing spills, or keeping them small, can spare companies the cost of a major cleanup, he said.
As an example, Schlagenhauf said one company has seen its spill numbers drop from 20 in 2015 to about six last year and one so far this year.
Oil and gas spills dropped from more than 700 in 2014 to 509 last year, a drop that may partly be because of reduced oil and gas development levels, but the commission also thinks may be because of its audit program.
Source: https://www.gjsentinel.com/news/articles/corrosion-causes-half-of-oil-gas-flowline-spills


Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...