ANSI / NACE MR0175 / ISO 15156 gives requirements and
recommendations for the selection and qualification of carbon
and low-alloy steels and corrosion-resistant alloys (CRAs) for
equipment in oil and gas production in H2S-containing
environments. When selecting a material that will be exposed to
H2S, the user can select CRAs from NACE MR0175 Part 3 Annex A
using the materials selection tables. This infographic analysis the
information shown in the material selection tables.
Subscribe to:
Post Comments (Atom)
[MW:35633] IP Joint
Hello experts, I would like to know what is IP joints in piping(31.3)? Regards Saurabh -- https://materials-welding.blogspot.com/...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment