Hi,
Please refer Sectuion VIII - Div.1 - UG 16 (c) - Mill under tolerance: 0.25mm or 6% of the thickness ordered. But in any case it should be more than the design thickness.

Thanks& Regards,

 

(Karthik)

Karthikeyan.S

QA/QC Manager
Agon Pacific Co.,Ltd.
M: +66-655-174-397, +66-892-512-282

E-mail : karthik6684@yahoo.com



On Thursday, January 25, 2018, 8:26:46 PM GMT+7, pradip kumar Sil <pradipsil@gmail.com> wrote:


Dear Everybody,
Can anybody inform me how much mill tolerance thickness is acceptable for Plate material with code reference as per ASME.
Thanks in advance.
Regards,
Pradip

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...