Skip to main content

[MW:27263] RE: 27256] Thickness of Painting (DFT)

Dear Karthikeyan,

When I assume what you mean by the datasheet is the project specification and it is mentioned Maximum 350 microns it's definitely a contract violation and may not be acceptable. Further for what standard to use is dependent on your project coating specification. However the most common is NACE/SSPC PA2. The standard calls for 3 readings should be taken within a circle of 1.5" dia and the average is called one spot; in your case the average of three readings should not be above 350microns ie the range of one spot should be 280~350micron (80%~100%). However practically its not possible that you get a reading like 1000 and still your average is 350%maximum. So this cannot be acceptable

Assuming that the data sheet of the paint material calls for 350microns maximum then you can not in any case cross the limit of manufacturer datasheet.

Further the defects due to high film thickness are dependent on the paint material; improper curing, cracks, checking, wrinkling or amine blush are few to name.

Your paint manufacturer may give you proper solution however in the most cases only solution is reblasting.

 

With best regards,

Umar

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Karthikeyan Muthuvel
Sent: Saturday, January 13, 2018 3:26 PM
To: materials-welding@googlegroups.com
Subject: [MW:27256] Thickness of Painting (DFT)

 

Dear Experts,

 

I'm very fresh for Painting Inspection, Kindly advise me for following 

 

In the data sheet it is mentioned maximum DFT  is 350 microns, when I measured on the piping its shows 1000 microns  and above, Please clarify is it acceptable or not which international standards should i follow and what are defect will occur due to the higher thickness of coating.

 

 Looking forward for yours kind valuable feedback.

 

Thanks & Warm Regards,


KARTHIKEYAN  M.

Mobile:+966-501176985,

P Save A Tree - Please do not print unless really need

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...