Wednesday, January 24, 2018

Re: [MW:27284] PQR PMI - Fe value

Its prob with instrument used for chemical analysis
Plz test with oes, inform lab to use calibration block for ni alloy (inconel 625) before testing
Yr specimen will be showing req values for %Fe

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...