Friday, January 19, 2018

Re: [MW:27269] Thickness of Painting (DFT)

Dear sir,

Higher DFT cause paint cracking after drying, Reason DFT shall controlled. 

Thanks & Regards

DINESH VITTHAL SOMWANSHI

BACHELOR IN MECHANICAL ENGINEER

AUTHORIZED PIPING / WELDING / NDT / PAINTING INSPECTION PERSONNEL
API 570 - Piping Inspector, AWS - CWI , CSWIP 3.1*,*BGAS  Gr 2 / 3
NDT II -UT , RT , MT , PT, VT
+7 924 374 6660 Russia , 00919881344135 India ( Whatsapp )
Skype = dinesh somwanshi

असो द्यावी दया तुमच्या लागतसे पाया.

*Pray for others, sometime, You might never need to pray for yourself
again.....*


On Tue, Jan 16, 2018 at 11:06 AM, Ramin Kondori <raminkondori@gmail.com> wrote:
Normally, it should be rejected. The norm for maximum applied paint (or each layer) is 2 times the specified DFT. But refer to paint manufacturer all the time. Though, some of them give you false assurances.

Ramin  Kondori
Sr. QA/QC & Welding Engineer
-----------------------------------------------------------
PG-Dip. in Welding Engineering (IWE  AT  0070)
BSc. in Civil Engineering (IUT)
BGAS Painting Inspector
ASNT Level I&II
                        

On Mon, Jan 15, 2018 at 4:58 PM, 'PRAMODH NAIR' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear Karthikeyan,

Refer your project specification/procedure, which standard to be followed. If nothing is mentioned, refer SSPC PA2. Its describe (Procedure) how you have to measure  the DFT. 

If the thickness is higher than what it is mentioned in the specification, always refer with coating manufacture/specifier/designer.

Regards,

Pramodh Ramanunny

If We Work With Determination And Perfection, Success Will Follow



On Monday, January 15, 2018, 3:38:35 PM GMT+3, Karthikeyan Muthuvel <m.karthick2020@gmail.com> wrote:


Dear Experts,

I'm very fresh for Painting Inspection, Kindly advise me for following 

In the data sheet it is mentioned maximum DFT  is 350 microns, when I measured on the piping its shows 1000 microns  and above, Please clarify is it acceptable or not which international standards should i follow and what are defect will occur due to the higher thickness of coating.

 Looking forward for yours kind valuable feedback.

Thanks & Warm Regards,

KARTHIKEYAN  M.
P Save A Tree - Please do not print unless really need

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...