[MW:27285] Welding of uPVC Profiles

Dear Experts,

I am welding uPVC profiles (Thickness 2-3 mm and width 65-70mm) for making doors & windows and after welding at corner joints, the joints are getting cracked at the corner.

The parameters which we are currently following are as follows:

Temp: 245+,- 5deg C
Welding Time: 30 sec
Heating time: 30 sec
Welding Pressure: 6 Bar
Clamping Pressure: 4.5bar

Please advice to join the crack free weld.

Thank you in advance.

With Kind Regards,

Amit Kumar Singh
Mob: +91-7898572921

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...