[MW:27280] RE: 27277] Mixture Gas Ar/N2

Abi,

 

If premixed gases are procured from reputed manufacturers , it should not be a concern. What's the gas mix: Ar+2% N2 or Ar+5%N2 ?

Higher percentage of Nitrogen in the gas mix may cause porosities in DSS welds. Also there are many other factors also, which could cause porosities in DSS welds. One has to see everything in totality.

 

Thanks.

 

P.Goswami.P.Eng, IWE.

Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@quickclic.net,pradip.goswami@gmail.com

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Welding and material
Sent: January 22, 2018 11:14 PM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:27277] Mixture Gas Ar/N2

 

My name is Abi, I've the problem about mixture gas Ar/N2, each my welder performed welding on te Material DSS which used mixture gas Ar/N2, always occured porosity on each welded. Does it mix gas can cause porosity defect ???????????????

Thanks

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


Virus-free. www.avg.com

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...