Tuesday, January 16, 2018

[MW:27265] Re: Thickness of Painting (DFT)

Dear Shri Karthi,
 Its a huge difference between required and observed. If it very localized reading then may be think off if this reading is in general then simply reject it. Higher the DFT more probability of Peeling off.

Regards
HNJ

On Monday, 15 January 2018 18:08:34 UTC+5:30, Karthikeyan Muthuvel wrote:
Dear Experts,

I'm very fresh for Painting Inspection, Kindly advise me for following 

In the data sheet it is mentioned maximum DFT  is 350 microns, when I measured on the piping its shows 1000 microns  and above, Please clarify is it acceptable or not which international standards should i follow and what are defect will occur due to the higher thickness of coating.

 Looking forward for yours kind valuable feedback.

Thanks & Warm Regards,

KARTHIKEYAN  M.
Mobile:+966-501176985,
P Save A Tree - Please do not print unless really need

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...