Saturday, January 13, 2018

[MW:27256] Thickness of Painting (DFT)

Dear Experts,

I'm very fresh for Painting Inspection, Kindly advise me for following 

In the data sheet it is mentioned maximum DFT  is 350 microns, when I measured on the piping its shows 1000 microns  and above, Please clarify is it acceptable or not which international standards should i follow and what are defect will occur due to the higher thickness of coating.

 Looking forward for yours kind valuable feedback.

Thanks & Warm Regards,

KARTHIKEYAN  M.
Mobile:+966-501176985,
P Save A Tree - Please do not print unless really need

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...