Re: [MW:26867] Query Regarding Heat Treatment of Test Specimen ucs-85

I have a 31.5mm plate, SA-517 Gr.70 with no heat treatment done at the plant, but it suffered PWHT by customer request. My question is: do I need to apply item UCS-85 (c) or item UCS-85 (f) I need to remove test specimens for simulating heat treatment?
Thank you.

Em segunda-feira, 18 de agosto de 2014 10:08:13 UTC-3, George Dilintas escreveu:

Yes
Best regards
Dr Georgios Dilintas
Authorized Nuclear Inspector
Authorized Inspector Supervisor
HBS Regional Technical Manager


  From: shaikh ahmed [ahmed...@gmail.com]
  Sent: 08/18/2014 12:47 PM ZE5B
  To: material...@googlegroups.com; Karthik <karth...@yahoo.com>; George Dilintas
  Subject: [MW:21651] Query Regarding Heat Treatment of Test Specimen ucs-85


Dear Sir,
 
Kindly Suggest.
 
if plate is normalized SA-516-70,dish head 2.1 is cold formed and then head is normalized due to extreme fiber elongation. do we need test secimens be tested to satisfy UCS-85?
 
waiting.
 
kind regds,
Shaikh Ahmed

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...