Hi,

 

As per QW 403.18 / QW 423. 1 – if you take qualification on P no 1 to P no 1, then the welder will be qualified for p no 1 to P. no 15F, 34, and 41 to 49

You can take the qualification on P no 1- no problem, it is acceptable.

 

However for P no 1 base material,  your consumable should be F43 for welder qualification, and if any F No changes then you have to see the QW 430 for the same for the permissible…

 

Hope it is clear to you.

 

Thanks & Regards,

Lakshman Kumar B,

+91 9440031459

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Vanchinath S.A.
Sent: Friday, October 6, 2017 7:58 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:26867] Welder qualification

 

Yes with F43 consumable.

 

On 5 Oct 2017 6:48 pm, "venkkatesh krishnan" <venkkateshkrishnan@gmail.com> wrote:

Dear Gentlemen,

 

I have to qualify welder with base material in my hand is P-1 to P-1, but but actual WPS done on P-1 to P-43 base material. May i proceed to qualify the welder based on this WPS?

 

Thanks in advance.

 

Regards, 

Venkkatesh Gopalakrishnan.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...