Re: [MW:26932] Alloy PMI after PWHT(piping)

Simple, Abdul.
If it does not pass in PMI, why would you send it for PWHT?
 
Best Regards,
Shashank C Vagal  
 


On Thursday, 19 October 2017 3:29 PM, abdulkhadar musthafa <abdulrilvan@gmail.com> wrote:


Dear Friends
   
Would Some one explain me  regarding Alloy materials(P11 and P5) having PWHT, but contractor side suggest they want to PMI before PWHT.
 I want is there is against code or mentioned in our codes.

waiting for reply 

--
ABDUL KHADAR MUSTHAFA
QC-WELDING INSPECTOR
+91-9841879981
"The reward of deeds depends upon the intentions"
"செயல்கள் அனைத்தும் எண்ணங்களைப் பொருத்தே அமைகின்றன. ஒவ்வொருவருக்கும் அவர் எண்ணியதே கிடைக்கிறது."


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...