Thursday, October 19, 2017

[MW:26931] RE: 26929] Alloy PMI after PWHT(piping)

You may read through API-RP-578, clause 4.0 and various associated sub-clauses. PWHT does not cause any major change in the alloy content of the base metals and the welds. Alloying elements may diffuse within the matrix, during PWHT, instead of being locally segregated. Thus the PMI results after PWHT could be more consistent than before PWHT. Although such changes could be very microscopic.

 

Design codes does not specify at what point such verification is to be done. It's clients' call.

 

If the PMI technique is XRF, it may be performed before or after PWHT.

If the technique is OES, then many clients prefer this before PWHT, as arcing during the OES process may leave arc stains/marks . Such marks  may require grinding of buffing, not usually desirable after PWHT, due to chances of human errors.

 

Thanks.

 

P.Goswami.P.Eng, IWE.

Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@quickclic.net,pradip.goswami@gmail.com

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of abdulkhadar musthafa
Sent: October 19, 2017 5:50 AM
To: materials-welding@googlegroups.com
Subject: [MW:26929] Alloy PMI after PWHT(piping)

 

Dear Friends

   

Would Some one explain me  regarding Alloy materials(P11 and P5) having PWHT, but contractor side suggest they want to PMI before PWHT.

 I want is there is against code or mentioned in our codes.

 

waiting for reply 

 

--

ABDUL KHADAR MUSTHAFA
QC-WELDING INSPECTOR
+91-9841879981
"The reward of deeds depends upon the intentions"
"செயல்கள் அனைத்தும் எண்ணங்களைப் பொருத்தே அமைகின்றன. ஒவ்வொருவருக்கும் அவர் எண்ணியதே கிடைக்கிறது."

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


Virus-free. www.avg.com

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...