Monday, October 16, 2017

Re: [MW:26912] using of ER308 filer.

Dear . you were using material grade of 316l for low temp with added Mo. Ni%.

Using lower grade of filler equivalancies 308 against 316L not acceptable.

Thanking You,

With Regards..
Dinesh V Somwanshi
Api 570, Cswip 3.1,Bgas 2
Authorised Certified Piping, Welding, Painting Inspector.
00919881344135

On Oct 16, 2017 11:17 AM, "'sangram routray' via Materials & Welding" <materials-welding@googlegroups.com> wrote:
Dear group members ;
our sub-contractor welded one joint  304 PIPE to 316L valve by ER308 filler but client said its not acceptable.
can some one help me regarding above mater .
is it Acceptable or not? 
Answerd with some code or standard reference. 
 
Thanks & Regards

Sangramkeshari Routaray
Welding inspector

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...